Specification and qualification of welding procedures for metallic materials ? Qualification based on pre-production welding test
This European Standard is a part of a series of standards, details of this series are given in EN ISO 15607:2003,
annex A.
This standard specifies how a preliminary welding procedure specification is qualified based on pre-production
welding tests.
The principles of this standard may be applied to other welding processes.
This standard is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction
welding of metallic materials.
The use of this standard can be restricted by an application standard or specification.
ΚΩΔΙΚΟΣ ΠΡΟΪΟΝΤΟΣ:
CYS EN ISO 15613:2004
This European Standard is a part of a series of standards, details of this series are given in EN ISO 15607:2003,
annex A.
This standard specifies how a preliminary welding procedure specification is qualified based on pre-production
welding tests.
The principles of this standard may be applied to other welding processes.
This standard is applicable to arc welding, gas welding, beam welding, resistance welding, stud welding and friction
welding of metallic materials.
The use of this standard can be restricted by an application standard or specification.